Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 GF50 HS L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UX06003 PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UX06003 is a compound based on Polyphalamide resin containing Carbon Fiber. Added features include Electrically Conductive, Mold Release, Heat Stabilized. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
Polyram Polytron P60B04-S Polypropylene, 60% Long Glass Fiber A chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Plenco 6500 Phenolic, Briquette, Transfer Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | |
3M Z100™ Restorative Dental Composite 3M™ Z100™ restorative is an all purpose, esthetic, light cured dental composite. 3M Restorative Z100 features a translucency and opalescence similar to that of natural teeth and is used for porce.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO Data |
BASF Ultramid® B3EG10 BK00564 50% Glass Filled PA6 (Dry) Ultramid B3EG10 BK00564 is a 50% glass fiber reinforced injection molding PA6 grade. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U.. |
|||
Flexural Modulus | 14.5 - 15.9 GPa | 2100 - 2300 ksi | |
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili.. |