Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
PolyOne Edgetek® NL-50GF/000 Black 13 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedBlackNylon 6/12 CompoundDry as Molded:PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific) LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A .. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF40 RM HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer Features: Heat Stabilized and Low Moisture AbsorptionAppearanc.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF44 HS X 44% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 44% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized TPCI# 95.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M15 HS L BK 40/15% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 15% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Ensinger Tecapeek® XP-114 Compression Molded PEEK Compound, 40% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | Tangent; ASTM D790 |
Applied Composites 8050 Polyester SMC Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: Radiant Panel, UL 94-VO, Low Shrink, PigmentableInformation provided by Applied Composites Corporation. |
|||
Flexural Modulus | 11.7 - 13.1 GPa | 1700 - 1900 ksi | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 686 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Modulus | 11.7 - 13.1 GPa | 1700 - 1900 ksi | |
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound BMC T10(GP) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T10(GP) is well suited for injection, transfer or compression molding of intricate parts... |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | Tangent, 0.125 in; ASTM D790 |
Matrixx Group 80M7451 45% Glass/Mineral Filled PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |