Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.84 GPa | 267 ksi | Tangent; ASTM D790 |
Multibase Nylex™ 2185 R15 Polyamide + PP Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho.. |
|||
Flexural Modulus | 1.84 GPa | 267 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Opnyl OP66UT108 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |
|||
Flexural Modulus | 1.84 GPa | 267 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 1.84 GPa | 267 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 1.84 GPa | 267 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT 4.2 specific gravity, PBT, gray |