Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.78 GPa | 258 ksi | ASTM D790 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | ASTM D790 |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | ASTM D790 |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | ASTM D790 |
Styrolution Terluran® EHI-4 NR ABS Extrusion Application Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | ISO 178 |
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | ASTM D790 |
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 1.78 GPa | 258 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS/PC 9801 Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc. |