Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.65 GPa | 239 ksi | ASTM D790 |
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware NatureWorks® PLA polymer AW 240D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed .. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Ravago Manufacturing Americas Hysun™ 383 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 1.65 - 6.21 GPa | 240 - 900 ksi | Average value: 1.94 GPa Grade Count:18 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Flexural Modulus | 1.65 - 12.0 GPa | 239 - 1740 ksi | Average value: 4.05 GPa Grade Count:5 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | |
Kraton® FG1901 + PBT blend (30/70) Blending KRATON FG polymers with PBT significantly improves the toughness. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second .. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000A PP LNP* STAT-KON* MD000A is a compound based on Polypropylene resin containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | ISO 178 |
Unipetrol PP MONSTEN® NB 108 Polypropylene Homopolymer Applications include injection molding and fibers. Basic and anti-gasfading stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman COMTUF® 420 Impact Modified PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | ASTM D790 |
Total PPC 4481WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4481WZ is a nucleated impact copolymer with a Melt Flow index of 4.0 g/10 min.TOTAL Polypropylene 4481WZ is characterized by a good stiffness/impact balance couple.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 5142K Extrusion - Sheet - Thermoforming Polypropylene HomopolymerApplications: Extrusion, Sheet and Thermoforming ApplicationsFormolene 5142K is a high viscosity homopolymer designed primarily for thermoformed cups and container applications. It contai.. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | 1.3 mm/min, tangent; ASTM D790 |
A. Schulman PP 3466-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3466-01 is a homopolymer polypropylene with the addition of antistatic. This product enhances processing with fast cycle times in injection molding.ApplicationPP 3466-01.. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | ASTM D790 |
Covestro Baydur® STR/F-275 IMR Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System Contains continuous strand fiberglass mat.0.0985 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem FT120WV Homopolymer Polypropylene Description: Antistatic, nucleated, good mold release.Applications: Suggested uses include cosmetic packaging, disposable cutlery, closures, overcaps.Process: Injection Molding.This resin meets the .. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | ASTM D790 |
Carmel Olefins CAPILENE® G 86 E Polypropylene Homopolymer CAPILENE® G 86 E is a polypropylene homopolymer intended for extrusion and thermoforming applications. This grade is formulated with a low water carry-over additive packaging and it exhibits good m.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
Asahi Kasei Thermylene® P-05FG-0870 5% Glass Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP1020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | SAE J949 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.65 GPa | 240 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Flexural Modulus | 1.65 GPa | 239 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |