Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.585 GPa | 229.9 ksi | ASTM D790 |
Eastman Tritan EX401 Copolyester Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | ASTM D790 |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | ASTM D790 |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | ASTM D790 |
Eastman Tritan MX811 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO.. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | ASTM D790 |
Eastman Tritan TX2000 Copolyester Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | ASTM D790 |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can.. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | chs 0.05 in/min; 1% secant; ASTM D790 |
Diamond Polymers NPP30-1200S Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 1.585 GPa | 229.9 ksi | ISO 178 |
Cathay PA511 Renewable Engineering Polyamide Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical pr.. |