Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.55 GPa | 225 ksi | |
Plastcom SLOVALEN PC 79 T 20 PP/C reinforced with 20% mineral filler Features: Modified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Antistatic agent. Delivered in natural mode and i.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent; ASTM D790 |
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ASTM D 790 |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Entec Hypel® PEHD.8/.962 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 1.55 GPa @Temperature 60.0 °C |
225 ksi @Temperature 140 °F |
ASTM D790 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
M. Holland Company PP400 Polypropylene Homopolymer Features: Medium Flow, General PurposeUses: Closures, Food Containers, Household Goods, VialsApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent-Method 1; ASTM D790 |
Ineos G60-25-144 HDPE Ineos G60-25-144 is a high density polyethylene homopolymer typically used in the production of sheet extrusion and blow molded containers. This material meets the Food and Drug Administration requ.. |
|||
Flexural Modulus | 1.55 GPa @Temperature 23.0 °C |
225 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H20Z-00 Polypropylene Homopolymer This is a nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Appl.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 17TOP BU is a black colored, 17% talc-filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-2120 17TOP BU is developed for producing injection .. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 1310 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | |
Kraton® FG1901 + PBT blend (30/70), Oven Aged Oven aged at 150°C (°F) for 2 hours. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second generation block polymers in whi.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade) ApplicationsPETROTHENE LM 6007-00 resin exhibits very low taste and odor characteristics as well as good rigidity. Typical applications include water, and milk and juice bottles.Regulatory StatusLM.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl RF1132 PPE+PP PPE+PP blend for high frequency applications. Good heat resistance and low DK.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP (Asia Pacific) LNP* Lubricomp* ML004S is a compound based on Polypropylene resin containing PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Eastman Tritan TX1000 Copolyester Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
CPC - Vycom HITEC® HDPE High Density Polyethylene Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent Method 1; ASTM D-790 |
Bapolene® 0760 Polyethylene, Blow Molding Grade This resin is a high density polyethylene homopolymer for blow molding applications. It is recommended for applications that require high top load strength and good stiffness. This product meets 2.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 107 Polypropylene Homopolymer Made for injection molding. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | tangent; ASTM D790 |
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP2030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |