Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.36 GPa | 197 ksi | ASTM D790 |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 1.36 GPa | 197 ksi | 1% Secant; ASTM D790 |
Flint Hills P4G2T-077D Homopolymer Polypropylene Homopolymer, FDA compliantFeatures: Antistat.Applications: Extrusion: straw grade.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Flexural Modulus | 1.36 GPa | 197 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Flexural Modulus | 1.36 GPa | 197 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Flexural Modulus | 1.36 GPa | 197 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Conditioned (2.5% Moisture) Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Flexural Modulus | 1.36 GPa | 197 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Conditioned (2.5% Moisture) Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Flexural Modulus | 1.36 - 3.38 GPa | 198 - 490 ksi | Average value: 2.11 GPa Grade Count:71 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |