Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
PolyMirae Moplen EP300K Injection Molding Grade Polypropylene Moplen EP300K is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300K is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
PolyMirae Moplen HP310R Extrusion Coating and Lamination Grade Polypropylene Moplen HP310R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP310R is a copolymer particularly suitable for extrusion coating and.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
PolyMirae Moplen RP340N Injection Molding Grade Polypropylene Moplen RP340N is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340N is a random copolymer particularly suitable for injecti.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
PolyMirae Moplen RP344R Injection Molding Grade Polypropylene Moplen RP344R is a nucleated polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP344R is a random copolymer particularly suitable for.. |
|||
Flexural Modulus | 1.23 GPa | 179 ksi | Tangent; ASTM D790 |
Multibase Nylex™ 2185 FR Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
PolyMirae Moplen EP401M Injection Molding Grade Polypropylene Moplen EP401M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP401M is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.23 GPa | 179 ksi | 1% Secant; 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
LyondellBasell Alathon® L5440 High Density Polyethylene ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
Hyosung Topilene J640A PP J640A Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporatio.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790A |
Ineos H03G-05 Polypropylene Homopolymer Grade H03G-05 is a polypropylene homopolymer designed for BOPP applications and meet the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.Applications:Food Packa.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D760 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D760 |
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer Features: SEETEC M1600 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1600 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D760 |
LG Chemical SEETEC M1700 Polypropylene Impact Copolymer Features: SEETEC M1700 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1700 exhibits a very high flowability and a good balance of stiffness and impact strength.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H5814J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P840J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance part.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P851JO Polypropylene Injection Molding Key Characteristics:Good processabilityHigh gloss and brightnessOdorlessSafe for food contactRecommended Applications:Clear food containerClear large size containerThin wall productsInformation prov.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra.. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | |
Zylog Hipolyene® 2530 DW Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.23 GPa | 178 ksi | |
Zylog Hipolyene® 4955 T Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |