Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.981 - 9.51 GPa | 142 - 1380 ksi | Average value: 3.93 GPa Grade Count:18 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Hyosung Topilene C600Y PP C600Y Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Hyosung Topilene R500F PP R500F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Hyosung Topilene R500S PP R500S Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.981 GPa @Thickness 3.20 mm |
142 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON PO6062 mPPO+CNT+CF+GF Description: Injection Molding, mPPO+CNT+CF+GF, High Strength, Heat StabilityApplication: ATM parts, LCD Cell TrayCAS No. 35134-01-4, 25038-54-4, 65997-17-3, 7440-44-0 and 7782-42-5Information provi.. |
|||
Flexural Modulus | 0.981 GPa @Thickness 6.40 mm |
142 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | Olsen Stiffness; ASTM D747 |
Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | Olsen Stiffness; ASTM D747 |
Global F-7000 High Density Polyethylene Description-high quality is suitable for blown film @wide range of size & thickness Applications-large & small rolled film, shopping bag, merchant bag, disposal waste bagInformation provided by Glob.. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | Olsen Stiffness; ASTM D747 |
Global J-1600 High Density Polyethylene Description-suitable for injection moldingApplications-household products, handy craft flowers, toys, stationaryInformation provided by Global Polymers Corporation. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | Olsen Stiffness; ASTM D747 |
Global J-2308 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
LG Chemical LUTENE-H XL1800 HDPE Description: LUTENE-H XL 1800 is a optimum materials for under-floor heating and drinking water pipe by RAM type extrusion. It is excellent product with long-term internal pressure creep property an.. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
LG Chemical SEETEC PB150 HDPE Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stre.. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | >= 0.981 GPa | >= 142 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H2001WC High Density Polyethylene Wire & Cable Grade Key Characteristics:Excellent environmental stress cracking resistance (ESCR), high mechanical properties, high speed extrusionRecommended Applications:Jacketing of fiber optical cablesJacketing of .. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chem.. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 0.981 GPa | 142 ksi | ASTM D790 |
LG Chemical LUTENE-H ME9180 HDPE Description: LUTENE-H ME9180 is mainly intended for injection molding of complicated parts. It has high productivity and good appearance.Applications: Complicated parts, light-weight household.CAS N.. |