Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.965 GPa | 140 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Multi-Pro® 0710 C Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | Tangent; ASTM D790 |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 20-1001 Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-0616 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR020N Polypropylene Random Copolymer COPYLENE® CR020N is a random copolymer formulated with advanced nucleator technology and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have exceptional gloss a.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Multibase Multi-Flex® D 6505 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInform.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Techmer ES HiFill FR® CONC HDPE FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Techmer ES HiFill FR® HDPE FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Techmer ES Statiblend® 02010 MB Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinfor.Features: ConductiveAppearance: BlackTPCI# 9125116Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Techmer ES Statiblend® 02056 BKN Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Techmer ES Statiblend® 02056 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9111116Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | 1% secant; ASTM D790 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D 790 |
Total 8183 HDPE, blow molding Applications: cosmetic bottles, pharmaceutical bottles, industrial product containers, chemical packaging, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals ac.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Formosa Plastics Formolene® HP4401 Pipe HDPE High Density Hexene CopolymerApplications: Potable water, industrial mining, oil and gas gatheringsFormolene HP4401 is a high performance copolymer that is designed for the most demanding requiremen.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp Applications:Tool handlesToys/sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clar.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | 2% Secant; ASTM D790 |
Chevron Phillips Marlex® HP132 High Density Polyethylene, Pressure Pipe Grade This high performance PE 4710 HDPE is tailored for the demands of pressure pipe applications that require:Excellent long-term hoop strengthSuperb resistance to slow crack growthExceptional resistanc.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | 2% Secant; ASTM D790B |
ExxonMobil HDPE HD 6605.70 High Density Polyethylene Copolymer Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers NPP20-1201CAS Random Copolymer Polypropylene (Clarified, with Antistat) Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TR3015WV2 High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight EPR phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Formosa Plastics Formolene® HP4306 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for l.. |
|||
Flexural Modulus | 0.965 GPa | 140 ksi | ASTM D790 |
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lids and over-capsFormolene LH5204 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as .. |
|||
Flexural Modulus | 0.965 - 3.10 GPa | 140 - 450 ksi | Average value: 1.67 GPa Grade Count:17 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |