Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.276 - 17.3 GPa | 40.0 - 2510 ksi | Average value: 2.63 GPa Grade Count:256 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
LyondellBasell Microthene® F FN51000 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
LyondellBasell Microthene® F FN51900 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 818-073 offers the high environmental stress crack resistance characteristics of linear low density polyethylene with the processing properties needed for blowmolding and e.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO X MB Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Techmer ES HiFill® LDPE 0098 S LE Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Heat StabilizerFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | 1% secant - machine direction; ASTM D882 |
A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-86-K986T-98 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | machine direction; ASTM D882 |
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In.. |
|||
Flexural Modulus | 0.276 GPa | 40.0 ksi | ASTM D790 |
Arkema Group PLATAMID® 8020 Copolyamide Platamid® 8020 is a transparent, thermoplastic copolyamide designed for conversion by standard molding or extrusion techniques.Information provided by Arkema Group |
|||
Flexural Modulus | 0.276 - 0.414 GPa | 40.0 - 60.0 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Flexural Modulus | 0.276 - 0.480 GPa | 40.0 - 69.6 ksi | Average value: 0.346 GPa Grade Count:11 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |