Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0830 GPa | 12.0 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® CHP-010 Thermoplastic Polyolefin
(discontinued **) Applications: Soft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-705 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Base resin for fully formulated low voltage cable i.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
3M Dyneon™ THV™ 200P Fluorothermoplastic, Powder Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
3M Dyneon™ THV™ 200G Fluorothermoplastic, Pellet Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | ASTM D790 |
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.0830 GPa | 12.0 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-702 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |