Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0190 GPa | 2.76 ksi | ASTM D790 |
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where.. |
|||
Flexural Modulus | 0.0190 GPa | 2.76 ksi | ASTM D790 |
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, .. |
|||
Flexural Modulus | 0.0190 - 0.0960 GPa | 2.76 - 13.9 ksi | Average value: 0.0561 GPa Grade Count:15 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Flexural Modulus | 0.0190 GPa | 2.76 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Flexural Modulus | 0.0190 - 0.0372 GPa | 2.76 - 5.40 ksi | Average value: 0.0274 GPa Grade Count:3 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu.. |