Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LG713 ABS, Low Gloss Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Izod Impact, Unnotched | 1.17 J/cm @Thickness 12.7 mm |
2.20 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ASTM D256 |
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Unnotched | 1.18 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.20 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Izod Impact, Unnotched | 1.17 J/cm @Thickness 12.7 mm |
2.20 ft-lb/in @Thickness 0.500 in |
CW, Cond E-48/50; ASTM D256 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |