| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical ER451 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability
Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 6.40 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.252 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical HF380G ABS, High Flow
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical HF380G ABS, High Flow
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 6.40 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.252 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical HF380U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical HF380U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical LG713 ABS, Low Gloss
Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 6.40 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.252 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by..
|
|||
| Izod Impact, Unnotched |
1.17
J/cm <br>@Thickness 12.7 mm
|
2.20
ft-lb/in <br>@Thickness 0.500 in
|
CW, Cond E-48/50; ASTM D256 |
|
Industrial Laminates/Norplex NP634 Laminate
Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and..
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 3.20 mm,<br> Temperature -20.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -4.00 °F
|
ASTM D256 |
|
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Izod Impact, Unnotched |
1.18
J/cm <br>@Thickness 3.20 mm,<br> Temperature -30.0 °C
|
2.20
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature -22.0 °F
|
ASTM D256 |
|
LG Chemical ER461 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
|
|||
| Izod Impact, Unnotched |
1.17
J/cm <br>@Thickness 12.7 mm
|
2.20
ft-lb/in <br>@Thickness 0.500 in
|
CW, Cond E-48/50; ASTM D256 |
|
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **)
Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f..
|
|||