Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.00 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
7.49 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 12.7 mm |
7.50 ft-lb/in @Thickness 0.500 in |
CW, E-48/50 |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
7.49 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Lubrizol Isoplast® 2540 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
7.49 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Lubrizol Isoplast® 2540 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |