Polymer Property : Izod Impact, Unnotched = 1.08 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.08 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
2.02 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability
Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 1.08 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
2.02 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 1.08 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
2.02 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 1.08 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
2.02 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
LG Chemical LG713 ABS, Low Gloss
Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical
Izod Impact, Unnotched 1.08 J/cm

@Thickness 12.7 mm
2.02 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
Industrial Laminates/Norplex NP310HT Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Designed to meet GE specification A19B15B1Thickness..
Izod Impact, Unnotched 1.08 J/cm

@Thickness 6.40 mm,
Temperature -20.0 °C
2.02 ft-lb/in

@Thickness 0.252 in,
Temperature -4.00 °F
ASTM D256
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Unnotched 1.08 J/cm

@Thickness 6.40 mm,
Temperature -20.0 °C
2.02 ft-lb/in

@Thickness 0.252 in,
Temperature -4.00 °F
ASTM D256
LG Chemical MA201 ABS, Low Gloss
Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical