Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.300 GPa @Temperature 121 °C |
43.5 ksi @Temperature 250 °F |
50%RH; ASTM D790 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.300 GPa @Temperature 80.0 °C |
43.5 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 0.300 GPa @Temperature 121 °C |
43.5 ksi @Temperature 250 °F |
ASTM D790 |
BASF Ultramid® 8281 HS GP PA6 (Dry) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |