Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.3 GPa @Temperature 216 °C |
2800 ksi @Temperature 420 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Flexural Modulus | 19.3 GPa @Temperature -53.9 °C |
2800 ksi @Temperature -65.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 19.3 GPa @Temperature 21.1 °C |
2800 ksi @Temperature 70.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 19.3 GPa @Temperature 93.3 °C |
2800 ksi @Temperature 200 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Modulus | 19.3 GPa @Temperature 23.9 °C |
2800 ksi @Temperature 75.0 °F |
Wet (2hr water boil); ASTM D790 |
Park Electrochemical Nelcote® P-600 Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160.. |
|||
Flexural Modulus | 19.3 GPa @Temperature 121 °C |
2800 ksi @Temperature 250 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® P-670I Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-670I is a versatile, non-styrenated/low VOC polyester resin. P670I is used in a wide variety of applications including radomes, tooling and aircraft structures.Key Features and Benefits:.. |
|||
Flexural Modulus | 19.3 GPa @Temperature 23.0 °C |
2800 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree.. |
|||
Flexural Modulus | 19.3 GPa @Thickness 1.57 mm |
2800 ksi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
Flexural Modulus | 19.3 GPa @Temperature 23.0 °C |
2800 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional .. |