Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.5 GPa @Temperature -40.0 °C |
2390 ksi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Modulus | 16.5 GPa @Temperature 80.0 °C |
2390 ksi @Temperature 176 °F |
Warp |
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26T/50%/7581 Glass Fabric 300 gsmInformation provided by HexCel |