Mechanical Properties Metric English Comments
Flexural Modulus 13.0 GPa

@Temperature 23.0 °C
1890 ksi

@Temperature 73.4 °F
ISO 178
Premix Premi-Glas® 1286 Glass Reinforced SMC
Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding..
Flexural Modulus 13.0 GPa

@Temperature -40.0 °C
1890 ksi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.25%); ASTM-D790
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 13.0 GPa

@Temperature -40.0 °C
1890 ksi

@Temperature -40.0 °F
Practical Use; ASTM-D790
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 13.0 GPa

@Temperature -40.0 °C
1890 ksi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 13.0 GPa

@Temperature 23.0 °C
1890 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.0%); ASTM-D790
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 13.0 GPa

@Temperature 250 °C
1890 ksi

@Temperature 482 °F
ISO 178
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound
BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri..