Mechanical Properties Metric English Comments
Flexural Modulus 11.7 GPa

@Temperature 93.3 °C
1700 ksi

@Temperature 200 °F
Dry; Post-Cure; ASTM D790
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Flexural Modulus 11.7 GPa

@Temperature 23.0 °C
1700 ksi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil..
Flexural Modulus 11.7 GPa

@Thickness 0.500 mm,
Temperature 22.0 °C
1700 ksi

@Thickness 0.0197 in,
Temperature 71.6 °F
secant; ASTM D790-1
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..
Flexural Modulus 11.7 GPa

@Temperature 23.0 °C
1700 ksi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber
Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s..
Flexural Modulus 11.7 GPa

@Temperature -40.0 °C
1700 ksi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.6%); ASTM-D790
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 11.7 GPa

@Thickness 0.500 mm,
Temperature 22.0 °C
1700 ksi

@Thickness 0.0197 in,
Temperature 71.6 °F
Secant; ISO 178
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo..
Flexural Modulus 11.7 GPa

@Temperature 23.0 °C
1700 ksi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved