Mechanical Properties Metric English Comments
Flexural Modulus 0.300 GPa

@Temperature 121 °C
43.5 ksi

@Temperature 250 °F
50%RH; ASTM D790
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Flexural Modulus 0.300 GPa

@Temperature 80.0 °C
43.5 ksi

@Temperature 176 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 0.300 GPa

@Temperature 121 °C
43.5 ksi

@Temperature 250 °F
ASTM D790
BASF Ultramid® 8281 HS GP PA6 (Dry)