Mechanical Properties Metric English Comments
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS
PC+ ABS General Purpose Non-FR
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS
PC+ ABS Automotive applications
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific)
PC+ ABS Automotive applications
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East)
PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging.
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 55.0 J

@Temperature 23.0 °C
40.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Copyright © lookpolymers.com All Rights Reserved