Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 47.0 J @Temperature -40.0 °C |
34.7 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature -30.0 °C |
34.7 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS Extrusion blowmolding grade. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature -30.0 °C |
34.7 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS (Asia Pacific) Extrusion blowmolding grade. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC Available in a wide range of colors. Recommended for unpainted exterior/high heat/high impact applications. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Asia Pacific) Weatherable, injection moldable ASA+PC blend. In a wide range of colors. Recommended for unpainted exterior/high heat applications. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature -40.0 °C |
34.7 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature -40.0 °C |
34.7 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 364 PBT+PC Designed for outdoor telecommunications enclosure applications. |