Mechanical Properties Metric English Comments
Dart Drop, Total Energy 44.0 J

@Temperature -20.0 °C
32.5 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Valox® 364 PBT+PC
Designed for outdoor telecommunications enclosure applications.
Dart Drop, Total Energy 44.0 J

@Temperature -30.0 °C
32.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Asia Pacific)
High modulus/impact/heat PPE+PP.
Dart Drop, Total Energy 44.0 J

@Temperature -30.0 °C
32.5 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX PPX7115F PPE+PP
High modulus/impact/heat PPE+PP. Compliant with US FDA food contact regulations for temperatures of use of room temperature and below.