Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Rupture Strength | 310 MPa @Temperature 705 °C, Time 360000 sec |
45000 psi @Temperature 1300 °F, Time 100 hour |
Initial Stress |
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Rupture Strength | 310 MPa @Temperature 704 °C, Time 3.60e+7 sec |
45000 psi @Temperature 1300 °F, Time 10000 hour |
Plate |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Rupture Strength | 310 MPa @Temperature 649 °C, Time 360000 sec |
45000 psi @Temperature 1200 °F, Time 100 hour |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |