Mechanical Properties Metric English Comments
50% Modulus 0.00640 GPa
0.928 ksi
ASTM D638
Toyobo PELPRENE™ P40H Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
50% Modulus 0.00640 GPa
0.928 ksi
ASTM D638
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
50% Modulus 0.00640 GPa
0.928 ksi
ASTM D638
Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
50% Modulus 0.00640 GPa
0.928 ksi
ASTM D638
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo.