Polymer Property : 50% Modulus = 0.00380 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.00380 GPa
0.551 ksi
DIN 53504
Lubrizol ESTANE® T5384 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00380 GPa
0.551 ksi
ASTM D412
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ..
50% Modulus 0.00380 GPa
0.551 ksi
DIN 53504
Lubrizol ESTANE® 58201 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00380 GPa
0.551 ksi
ASTM D412; ASTM D638
Lubrizol Estane® 58201 Thermoplastic Polyurethane
Type: Estane® 58201 is an 82A Polyether-type thermoplastic polyurethane (TPU) compound.Features: Tear resistant properties.Uses: Injection Molding and general extrusion techniques.Available in Euro..
50% Modulus 0.00380 GPa
0.551 ksi
DIN 53504
Lubrizol ESTANE® 58561 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
50% Modulus 0.00380 GPa
0.551 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4520 Molded Brake Part
FormulationNordel® IP 4520
50% Modulus 0.00380 GPa
0.551 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR8020 Standard Adipate Ester Polyurethane
The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGr..