Lubrizol Estane® 58201 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® 58201 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type: Estane® 58201 is an 82A Polyether-type thermoplastic polyurethane (TPU) compound.Features: Tear resistant properties.Uses: Injection Molding and general extrusion techniques.Available in Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength 39.0 MPa
5660 psi
ASTM D412; ASTM D638
Elongation at Break 680 %
680 %
ASTM D412; ASTM D638
50% Modulus 0.00380 GPa
0.551 ksi
ASTM D412; ASTM D638
100% Modulus 0.00460 GPa
0.667 ksi
ASTM D412; ASTM D638
300% Modulus 0.00710 GPa
1.03 ksi
ASTM D412; ASTM D638
Rebound 1.0 %
1.0 %
DIN 53512
Tear Strength 44.0 kN/m
251 pli
Die C; ASTM D624
Abrasion 43
43
mm<sup>3</sup>; DIN 53516
Compression Set 28 %

@Temperature 23.0 °C,
Time 79200 sec
28 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
71 %

@Temperature 70.0 °C,
Time 79200 sec
71 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -70.0 °C
-94.0 °F
DIN 53546