Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 5800 MPa | 841000 psi | ISO 899-1 |
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules |
|||
Tensile Creep Modulus, 1000 hours | 5800 MPa | 841000 psi | ISO 899-1 |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Tensile Creep Modulus, 1000 hours | 5800 MPa | 841000 psi | ISO 899-1 |
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance |
|||
Tensile Creep Modulus, 1000 hours | 5800 MPa | 841000 psi | ISO 899 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |