Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 2200 - 2600 MPa | 319000 - 377000 psi | Average value: 2450 MPa Grade Count:8 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Tensile Creep Modulus, 1000 hours | 2200 - 3180 MPa | 319000 - 461000 psi | Average value: 2520 MPa Grade Count:4 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Tensile Creep Modulus, 1000 hours | 2200 MPa @Time 3.60e+6 sec |
319000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Creep Modulus, 1000 hours | 2200 MPa | 319000 psi | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Tensile Creep Modulus, 1000 hours | 2200 MPa | 319000 psi | |
BASF Polystyrol® 144 C Polystyrene (Europe) Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1000 hours | 2200 MPa | 319000 psi | |
BASF Polystyrol® 143 EO Polystyrene (Europe) Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1000 hours | 2200 MPa @Strain <=0.500 % |
319000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |