Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 7500 - 12000 MPa | 1.09e+6 - 1.74e+6 psi | Average value: 9170 MPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa @Temperature 23.0 °C |
1.09e+6 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 - 15800 MPa | 1.09e+6 - 2.29e+6 psi | Average value: 11800 MPa Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa @Strain <=0.500 % |
1.09e+6 psi @Strain <=0.500 % |
ISO 899-1 |
Styrolution Luran® 378 P G7 35% Glass Filled SAN Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa | 1.09e+6 psi | ISO 899-1 |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa @Time 3.60e+6 sec |
1.09e+6 psi @Time 1000 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa | 1.09e+6 psi | ISO 899-1 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa @Strain <=0.500 % |
1.09e+6 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa @Strain <=0.500 % |
1.09e+6 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa | 1.09e+6 psi | ISO 899 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Creep Modulus, 1000 hours | 7500 MPa @Strain <=0.500 % |
1.09e+6 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |