Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 6100 MPa
885000 psi
ISO 899-1
Lanxess Pocan® T 7323 000000 PBT + PET, 20% Glass Fiber
PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load
Tensile Creep Modulus, 1000 hours 6100 MPa
885000 psi
ISO 899-1
Lanxess Pocan® T 7323 POS151 000000 PBT + PET, 20% Glass Fiber
PBT+PET, 20% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized
Tensile Creep Modulus, 1000 hours 6100 MPa
885000 psi
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced
General-purpose grade with 30% glass fiber for parts requiring especially good resistance to heat deformation.Applications: parts for hot-water contact, pump housings, fan blades.Data was collected ..
Tensile Creep Modulus, 1000 hours 6100 - 15000 MPa
885000 - 2.18e+6 psi
Average value: 10300 MPa Grade Count:8
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..