Secant Modulus, TD 2.275 - 3.28 GPa
330.0 - 476 ksi
ASTM D882
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Secant Modulus, TD 2.275 - 3.28 GPa
330.0 - 476 ksi
ASTM D882
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, TD 2.41 - 3.28 GPa
350 - 476 ksi
ASTM D882
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..