Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | at 1%; ASTM D882 |
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | ASTM D882 |
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | ASTM D882 |
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b.. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | ASTM D882 |
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic.. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | ASTM D882 |
Chevron Phillips 5497 LDPE High Clarity, Bakery Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Openability, Suited for High Speed Converting, Good Clarity. Slip 1000 ppm. Antiblock 10000 ppm.Applications:Bakery Film, Bread BagsProcessing Con.. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | 0.01; ASTM D882 |
Eastman E6838-902F Polyethylene Film
(discontinued **) Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business .. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | 1% Secant; ASTM D882 |
Eastman 1830F Polyethylene
(discontinued **) Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and.. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | 1% Secant; ASTM D882 |
Eastman E6838-922F Polyethylene
(discontinued **) E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat.. |
|||
Secant Modulus, TD | 0.240 GPa | 34.8 ksi | 1% Secant; ASTM D882 |
Eastman E6838-964F Polyethylene
(discontinued **) E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |