Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.186 GPa | 27.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Secant Modulus, TD | 0.186 GPa | 27.0 ksi | ASTM D882 |
Huntsman PE1068 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21.. |
|||
Secant Modulus, TD | 0.186 GPa | 27.0 ksi | Film value |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Secant Modulus, TD | 0.186 GPa | 27.0 ksi | Film value |
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Secant Modulus, TD | 0.186 GPa | 27.0 ksi | ASTM D882 |
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali.. |
|||
Secant Modulus, TD | 0.186 GPa | 27.0 ksi | ASTM D882 |
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr.. |