Mechanical Properties Metric English Comments
Secant Modulus, TD 2.275 - 3.45 GPa
330.0 - 500 ksi
ASTM D882
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..
Secant Modulus, TD 2.59 - 3.45 GPa
376 - 500 ksi
ASTM D882
Honeywell Capran® Emblem™ 1200Matte Matte Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1200Matte is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats,..
Secant Modulus, TD 2.275 - 3.45 GPa
330.0 - 500 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Secant Modulus, TD 2.275 - 3.45 GPa
330.0 - 500 ksi
ASTM D882
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..