Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.110 GPa | 16.0 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Secant Modulus, TD | 0.110 GPa | 16.0 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut.. |
|||
Secant Modulus, TD | 0.110 GPa | 16.0 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Secant Modulus, TD | 0.110 GPa | 16.0 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Secant Modulus, TD | 0.110 GPa | 16.0 ksi | ASTM D882 |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |
|||
Secant Modulus, TD | 0.110 GPa | 16.0 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol.. |
|||
Secant Modulus, TD | 0.110 GPa | 16.0 ksi | ASTM D882 |
M. Holland Company LL217AA LLDPE
(discontinued **) Features: High Clarity, Copolymer, Good ProcessabilityUses: Film, Cast FilmApprovals: FDA 21 CFR 177.1521Processing Method: Blown Film and Cast FilmInformation provided by M. Holland. |