Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.60 GPa | 232 ksi | ASTM D882 |
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T.. |
|||
Secant Modulus, MD | 1.60 GPa | 232 ksi | ISO 527-3 |
Borealis Bormod™ HD905CF Polypropylene Homopolymer for Cast Film Bormod HD905CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, suitable for the manufacturing of unoriented film on chill roll process. It is recomme.. |
|||
Secant Modulus, MD | 1.60 GPa | 232 ksi | ISO 527-3 |
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is s.. |
|||
Secant Modulus, MD | 1.60 GPa | 232 ksi | ASTM D882 |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |