Mechanical Properties Metric English Comments
Secant Modulus, MD 0.965 - 1.103 GPa
140 - 160.0 ksi
ASTM D882
Honeywell ACLAR® 22A (2.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide..
Secant Modulus, MD 0.965 - 1.103 GPa
140 - 160.0 ksi
ASTM D882
Honeywell ACLAR® 22A (1.50 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide..
Secant Modulus, MD 0.965 GPa
140 ksi
ASTM D882
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used..
Secant Modulus, MD 0.965 GPa
140 ksi
ASTM D882
ExxonMobil Escorene® HD-7000F HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7000F exhibit excellent impact and toughness properties as well as high stiffness..
Secant Modulus, MD 0.965 GPa
140 ksi
ASTM D882
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness...