Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.138 - 0.172 GPa | 20.0 - 24.9 ksi | ASTM D882 |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Secant Modulus, MD | 0.138 GPa | 20.0 ksi | 2% Secant; ASTM D882 |
Dow DAF 780 Carpet Underlayment Adhesion Film DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow |
|||
Secant Modulus, MD | 0.138 GPa | 20.0 ksi | 2% Secant; ASTM D882 |
Dow INTEGRAL™ 933 Tough Film for Lamination to Porous Substrates INTEGRAL 933 Adhesive Film has a low melting, high flow adhesive layer that is useful for bonding to substrates such as polyurethane or polyethylene foam, or to non-woven textiles.Information provid.. |
|||
Secant Modulus, MD | 0.138 GPa | 20.0 ksi | 2% Secant; ASTM D882 |
Dow INTEGRAL™ 899A Monolayer Adhesive Film INTEGRAL 899A Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Glass, Polyurethane Foams/Sheet, Acrylic Adhesives, Wood.. |
|||
Secant Modulus, MD | 0.138 GPa | 20.0 ksi | ASTM D882 |
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A.. |
|||
Secant Modulus, MD | 0.138 - 0.234 GPa | 20.0 - 33.9 ksi | Average value: 0.182 GPa Grade Count:12 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Secant Modulus, MD | 0.138 GPa | 20.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |