Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 65.5 MPa | 9500 psi | Conditioned; ASTM D732 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Shear Strength | 65.5 MPa | 9500 psi | Interlaminar; ASTM D5379 |
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert.. |
|||
Shear Strength | 65.5 - 79.0 MPa | 9500 - 11500 psi | Average value: 72.2 MPa Grade Count:3 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Shear Strength | 65.5 MPa @Thickness 15.7 mm |
9500 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Shear Strength | 65.5 MPa | 9500 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Shear Strength | 65.5 MPa | 9500 psi | ASTM D732 |
PolyOne Edgetek® NI-20GF/000 Nylon 6/10, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |