Shear Strength 0.621 MPa
90.0 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/4-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-10 - 3/8 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-10/OX - 1/4 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, W Direction, min, preliminary value obtained at .500 inch thickness
Hexcel® HexWeb® HRH-327 - 3/16 - 4.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, W Direction
Hexcel® HexWeb® HRH-78 - 1/8 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP/F50 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR III 1/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR III 3/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 3/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-10 - 1/2 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 1/4 - 3.1 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.621 MPa
90.0 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-10 - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-10 - 3/16 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength >= 0.621 MPa
>= 90.0 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10/F35 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength 0.621 MPa
90.0 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Neoprene/Steel
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 0.621 MPa
90.0 psi
Overlap, LD Polyethylene
3M 5010 Polyurethane Multi-Purpose Adhesive
3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, f..
Shear Strength 0.621 MPa
90.0 psi
Overlap, Polypropylene
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M