Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 0.414 MPa | >= 60.0 psi | |
Parker Chomerics Tecknit® 0036 Two Part Flexible Adhesive-Sealant Silver-Glass Silicone Description: TECKNIT 0036 is an electrically conductive, medium viscosity, RTV silicone adhesive-sealant. This silver-plated glass filled system is formulated with a special conductive material pro.. |
|||
Shear Strength | >= 0.414 MPa | >= 60.0 psi | Cured; ASTM D1002 |
Parker Chomerics Tecknit CON/RTV-II 2 Part Silver Filled RTV Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | |
Shin-Etsu Silicones KE-3475TUV Silicone, RTV Conformal Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 1/4-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 0.414 MPa | >= 60.0 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 3/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 0.414 MPa | >= 60.0 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRH-10 - 3/16 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Plate Shear, L Direction |
Hexcel® HexWeb® HRH-78 - 3/8 - 1.5 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 0.414 MPa | >= 60.0 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 1/4-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 0.414 MPa | >= 60.0 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/16 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Overlap, Polypropylene |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |
|||
Shear Strength | 0.414 MPa @Time 3600 sec |
60.0 psi @Time 1.00 hour |
Aluminum, Overlap |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Overlap, Stainless Steel, 50% RH |
3M PN8017 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Overlap, Stainless Steel, 50% RH |
3M PN8019 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Overlap, Stainless Steel, 50% RH |
3M PN8027 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.414 MPa | 60.0 psi | Overlap, Stainless Steel, 50% RH |
3M PN8029 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |