Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 90.0 MPa | 13100 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Shear Strength | 90.0 MPa | 13100 psi | |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Shear Strength | 90.0 MPa @Temperature 23.0 °C |
13100 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, TSR9120 Carbon Tape Fiber: Toray® T700SInformation provided by HexCel |
|||
Shear Strength | 90.0 MPa | 13100 psi | In-Plane; After ageing at 70°C / 95% RH; RT |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Shear Strength | 90.0 MPa | 13100 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
Shear Strength | 90.0 MPa | 13100 psi | ASTM D732 |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |