Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 79.0 MPa | 11500 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Shear Strength | 79.0 MPa | 11500 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Shear Strength | 79.0 MPa | 11500 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Shear Strength | 79.0 MPa | 11500 psi | IL; After ageing at 70°C / 95% RH; RT |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Shear Strength | 79.0 MPa | 11500 psi | In-Plane, RT, Dry; EN6031 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |
|||
Shear Strength | 79.0 MPa | 11500 psi | ASTM D732 |
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Shear Strength | 79.0 MPa | 11500 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi.. |