Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 24.1 - 26.9 MPa | 3500 - 3900 psi | |
ND Industries 388 Toughened Instant Superglue Black toughened Cyanoacrylate for metal, rubber, and plastic |
|||
Shear Strength | 24.1 - 31.7 MPa | 3500 - 4600 psi | |
ND Industries 541 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, cams, collars, flywheels, rotors to shaft |
|||
Shear Strength | 24.1 - 31.7 MPa | 3500 - 4600 psi | |
ND Industries 542 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III |
|||
Shear Strength | 24.1 - 26.9 MPa | 3500 - 3900 psi | |
ND Industries Toughened Ethyl SuperGlue 310 Black flexible Cyanoacrylate for metal, rubber, and plastic |
|||
Shear Strength | 24.1 MPa | 3500 psi | |
NextGen Adhesives G907-32 Structural Adhesive Description: NGAC G907-32 is a thixotropic, epoxy adhesive system utilized extensively in staking, as well as, other industrial and structural applications.Advantages and Applications: The NGAC G907.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | |
Resinlab® RC8040 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Shear Strength | 24.1 MPa | 3500 psi | |
Resinlab® RC8060 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Shear Strength | 24.1 MPa | 3500 psi | |
Resinlab® RC8075 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Shear Strength | >= 24.1 MPa | >= 3500 psi | Tensile, Al to Al |
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Etched Aluminum |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Shear Strength | 24.1 MPa @Temperature 21.0 °C |
3500 psi @Temperature 69.8 °F |
Overlap |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Aluminum Oakite degrease |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, CRS Oakite degrease |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 24.1 MPa @Temperature -55.0 °C |
3500 psi @Temperature -67.0 °F |
Aluminum Overlap |
3M Scotch-Weld™ DP405 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Aluminum -etched/oily |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Etched Alum (oily) 49°C/100% RH/4 wks |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Stainless Steel, Cohesive Failure |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, CRS, Cohesive Failure |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Oily CRS, Cohesive Failure |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Aluminum, Cohesive Failure |
3M Scotch-Weld™ DP8805NS Low Odor Acrylic Adhesives 3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and .. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Stainless Steel (MEK/abrade/MEK), Cohesive failure/Adhesive Failure; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Etched Aluminum, Gasoline at RT for 30 days immersion, Cohesive Failure |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 24.1 MPa @Temperature -53.0 °C |
3500 psi @Temperature -63.4 °F |
Overlap |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Al-MEK/Abrade/MEK, Cohesive Failure |
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Aluminum, etched, Overlap, 30 day 65°C/80% RH, Cohesive Failure |
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of.. |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Etched Al, Air at 149°C for 40 days |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 24.1 MPa @Temperature 82.0 °C |
3500 psi @Temperature 180 °F |
Overlap; ASTM D1002 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Shear Strength | 24.1 MPa @Temperature -55.0 °C |
3500 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Shear Strength | 24.1 MPa | 3500 psi | Overlap, Methyl Ethyl Ketone immersion, RT for 30 days |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 24.1 - 31.7 MPa | 3500 - 4600 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT35 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |