Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 19.3 MPa | 2800 psi | ASTM D732 |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Shear Strength | 19.3 MPa @Temperature 23.0 °C |
2800 psi @Temperature 73.4 °F |
|
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive Mix ratio 2 to 1 by volume.TIGA 142-EX is a medium viscosity, sag resistant epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance is desired. Thi.. |
|||
Shear Strength | >= 19.3 MPa | >= 2800 psi | Al/Al, bond |
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien.. |
|||
Shear Strength | >= 19.3 MPa | >= 2800 psi | Bond, Al to Al |
Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures Description: Master Bond EP33CLV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and excel.. |
|||
Shear Strength | >= 19.3 MPa | >= 2800 psi | Al/Al, Tensile lap |
Master Bond EP21CLV Two Component Epoxy System Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Lap Shear; ASTM D1002 |
CoorsTek Epoxy Seal 216 (ES-216) B-staged epoxy lids ES-216 is available for applications where high strength and moisture resistance are required. It displays fillet formation characteristics and, after cure, is highly temperature and moisture resist.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Lap shear strength |
BCC Products BC 5200 Kwik-Set Adhesive BC5200 is a medium viscosity fast gelling two part Epoxy Adhesive System. With an easy to use 1 to 1 mix ratio, BC5200 is considered an excellent general purpose adhesive for in-shop use. BC5200 wil.. |
|||
Shear Strength | 19.3 - 19.48 MPa | 2800 - 2825 psi | Tensile Shear Adhesion |
3M Scotchkote™ FG 502 Epoxy Metal Repair Scotchkote Epoxy Metal Repair FG 502 has been specifically developed as a 100% solids epoxy coating for resurfacing and reforming metal machinery and equipment. It also combines good application cha.. |
|||
Shear Strength | 19.3 - 19.48 MPa | 2800 - 2825 psi | Tensile Shear Adhesion |
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Tensile Shear Adhesion |
3M Scotchkote™ HTX 517 Epoxy HT Lining Scotchkote Epoxy HT Lining HTX 517 has been specifically developed as a 100% solids epoxy coating for resurfacing and lining equipment operating at high temperatures.Product Features:Combines good a.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, CRS MEK/abrade/MEK |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, Cold Rolled Steel |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, Control |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, CRS/CRS tested after RT aging |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, Etched Aluminum-Cohesive Failure; ASTM D1002 |
3M Scotch-Weld™ LSB90 Flexible Epoxy 3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | ASTM D1002-94 |
Aremco Aremco-Bond™ 526N High Performance Epoxide Clear-Amber, 1:1 System for Tough Bonding Applications Also available filled with aluminum oxide (Alumina) or pigments |
|||
Shear Strength | 19.3 MPa @Temperature 120 - 122 °C |
2800 psi @Temperature 248 - 252 °F |
Average |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 19.3 MPa @Temperature -55.0 °C |
2800 psi @Temperature -67.0 °F |
Aluminum, etched, Overlap, Cohesive Failure |
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, grit-blasted steel; ASTM D1002 |
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, Aluminum; ASTM D1002-64 |
3M Scotch-Weld™ CA4 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Fast setting for a variety of plastics and rubbers.Information provided by 3M |
|||
Shear Strength | 19.3 MPa | 2800 psi | Overlap, Brass MEK/abrade/MEK |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 19.3 - 31.7 MPa | 2800 - 4600 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT80 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |